A new study has examined whether four commercial natural pigments can be compounded into biodegradable polyesters without losing their colour or disrupting processing, and found that most pigment–polymer pairs survive extrusion while long-term light stability remains the main obstacle.
The work, titled “Sustainability in the Development of Natural Pigment-Based Colour Masterbatches and Their Application in Biopolymers,” used blue spirulina, yellow curcumin, red beetroot and green chlorophyllin. Each pigment was combined with polylactic acid (PLA) and polybutylene succinate (PBS) to produce colour masterbatches on a twin-screw extruder. The formulations also contained titanium dioxide, calcium carbonate and stearic acid, added to support UV protection, pigment dispersion and processing.
Thermal limits define the processing window
Natural colorants are organic and can begin to degrade at temperatures below those needed to melt the carrier polymers, so the researchers first established thermal stability. Thermogravimetric analysis put degradation onset at approximately 229 °C for spirulina, 244 °C for curcumin, 258 °C for chlorophyllin and 267 °C for beetroot. PLA and PBS degrade at considerably higher temperatures.
The team then selected temperature profiles that melted each polymer while limiting heat exposure to the pigments: 145 °C for PBS and 190 °C for PLA. The twin-screw extruder ran at 65 rpm with a feed rate of 2 kg/h. Masterbatches were subsequently diluted into the matching matrix at 2, 4 and 6 wt%, and test specimens were produced by injection moulding.
Spirulina fails in PLA
Most pigment–polymer combinations processed successfully, but spirulina was the clear exception. During PLA compounding it lost its characteristic blue colour, which ruled out a blue PLA masterbatch. PBS, processed at the lower 145 °C, retained sufficient pigment stability for the combination to work. The result shows that pigment compatibility depends strongly on the thermal processing requirements of the specific polymer matrix.
Limited effect on flow and mechanics
Rheology changed only modestly. Neat PLA showed a melt flow rate of about 50 g/10 min, and the natural-pigment masterbatches stayed close to that value. PBS responded similarly, with a minor reduction in melt flow rate that points to a slight increase in melt viscosity.
That matters for compounders: a colour system offers little practical value if it forces major changes to screw design, pressure settings or moulding conditions. In this study, conventional twin-screw compounding and injection moulding handled most formulations without significant problems.
Mechanical testing covered the full 2 to 6 wt% addition range. PLA started from a Young's modulus of about 1710 MPa and tensile strength of 65.6 MPa; PBS from about 392 MPa and 34.5 MPa respectively. Coloured formulations stayed close to those baselines, and impact strength remained within a similar range, although individual pigments produced some variation.
Colour fastness is the weak point
Successful extrusion did not translate into durable colour. After 50 hours of xenon-lamp exposure, most formulations exceeded a colour difference of ΔE* = 2, the threshold for a visually perceptible change. The best performer was the PLA formulation containing 2 wt% green chlorophyllin masterbatch, which remained the main exception.
The authors therefore identify UV stability as the largest barrier to broader use. Packaging, consumer products, agricultural parts and outdoor applications would likely require additional stabilisation, protective coatings or pigment modification before natural colours can compete with conventional systems over long service periods.
Lower carbon footprint
The environmental comparison favoured the natural route. Under the study's assumptions, 1 kg of curcumin pigment corresponded to about 0.04 kg CO2-eq, against 18.65 kg CO2-eq for the inorganic green reference pigment. The natural-pigment masterbatches also consumed less electricity during extrusion and pelletising.
The researchers conclude that further development is still needed, particularly in lightfastness and thermal stability, but that several natural colorants can already be compounded into PLA and PBS on conventional equipment with only limited changes in melt viscosity and mechanical performance. Future work, they suggest, should focus on improving colour stability both during processing and during subsequent service exposure.