AMiquam Reports 0.1 mm In-Situ Defect Detection in LPBF Thin Walls

The Swiss company's recoater-mounted eddy current sensor scans each layer and maps indications to part coordinates, with results for thin walls and aeroengine blades.

Selin AydinNovember 24, 20265 min read1 views

A cutaway concept view of a metal LPBF machine, where a recoater-mounted sensor scans a fresh powder layer and maps indications onto a thin-walled part.

Swiss technology company AMiquam says it has improved the sensitivity of its in-situ eddy current inspection method for metal additive manufacturing, detecting flaws as small as 0.1 mm in thin-walled laser powder bed fusion (LPBF) parts. The company described the work in a technical publication ahead of Formnext 2026. The aim is to check parts layer by layer during the build, rather than relying only on post-build non-destructive testing.

The system places an eddy current sensor in the recoater assembly of an LPBF machine. As the recoater spreads powder across the build platform, the sensor scans the newly deposited layer and records electromagnetic signals that may indicate internal defects. AMiquam then maps the inspection data to the component geometry, so anomalies can be located and reported automatically.

Thin-wall test detects 0.1 mm holes

In one test, AMiquam used a 316L stainless steel specimen with a 0.7 mm wall thickness. It introduced five holes with diameters from 0.1 mm to 0.5 mm. Both through-holes and blind holes produced distinct peaks in the eddy current signal, the company says, and even the smallest 0.1 mm feature could be distinguished from background signal variation. The measurements covered about 127 layers, with each hole generating a corresponding signal peak as the build progressed.

According to AMiquam, the results point to potential inspection of complex structures such as triply periodic minimal surface (TPMS) heat exchangers. Such parts have internal channels and thin walls that can make conventional post-process inspection difficult. The company also described a concept for an inspection certificate that would record material, layer coverage, detection limits and detected indications. It said the certificate shown in the publication is illustrative, not an actual component certification.

Aeroengine blade case shows limits

A second application concerns LPBF-made aeroengine blades. In the described design, a conformal laser scanning strategy is used for the surface skin, while the bulk material is built with a conventional chessboard scanning approach. Those different strategies create different microstructures, which in turn affect eddy current signals.

AMiquam reports detection capability of about 0.2 mm in the conformal skin. In the bulk material, the threshold is about 0.5 mm, because microstructural variation adds signal fluctuations that make smaller indications harder to distinguish. The company says sensitivity depends on material characteristics, laser scanning strategy and component geometry, and that optimizing laser strategies could improve performance in bulk regions.

Mapping defects in three dimensions

The technology is also intended to locate defects precisely, not just flag process instability. Eddy current signals from each recoating pass are mapped onto the part geometry. Software then identifies indications above predefined thresholds and assigns X, Y and build-layer coordinates. That spatial record could help manufacturers investigate where defects occur and their possible origin. Capturing data throughout the build could also give earlier warning of quality issues instead of revealing them only after completion.

Quality assurance close to the build

AMiquam says the latest results show potential for eddy current inspection to become part of metal additive manufacturing quality assurance. Inspecting every layer and finding relatively small defects could be valuable for complex internal geometries and safety-critical parts. In aerospace, energy and medical manufacturing, where qualification and traceability matter, inspection evidence generated during production could reduce reliance on time-consuming post-build inspection.

The company cautions that detection thresholds remain dependent on geometry, material and manufacturing parameters. The reported figures should therefore be viewed as application-specific rather than universal performance limits. AMiquam’s work illustrates how established non-destructive testing principles can be adapted for in-process inspection, bringing defect detection, process understanding and quality documentation closer to the point of manufacture.